> Graham Motzing wrote:
> -------------------------------------------------------
> We had a couple places in Milwaukee I talked to years ago that did
> chrome and hard chrome, none of them had the plasma deposition process
> needed for plating to aluminum.
>
> Millennium technology in Plymouth, WI is the only place that would hone
> a moped size cylinder, they only wanted 175 back in 2012 but people are
> telling me they are closer to 300 now.
>
> Hopefully Jurrian will post what he finds with European suppliers. We
> are a ways off from that just yet
Here in the Netherlands there are different nikasil plating companies, all average about 200-250 euro per cylinder.